Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

Anticorodal 100/112

Bar

EN AW-6082, EN AlSi1MgMn, EN AlMgSi1, DIN 3.2315

DIN EN 573-3, DIN EN 754-2, DIN EN 754-3, DIN EN 755-2, DIN EN 755-3, DIN EN 515

Decoltal 500 / Aludur D202

Bar

EN AW-2011, EN AlCu6BiPb, EN AlCuBiPb, EN AW-2030, EN AlCu4PbMg, EN AlCuMgPb, DIN 3.1655

DIN EN 573-3, DIN EN 754-2, DIN EN 754-3, DIN EN 755-2, DIN EN 755-3, DIN EN 515

EN AW-1050A

Wire

EN AW-1050A, EN Al99.5, DIN 3.0255

DIN EN 573-3, DIN EN 1301/2, DIN EN 1301/3

EN AW-2030

Bar

EN AW-2030, EN AlCu4MgPb, AA 6026

EN AW-6026

Bar

EN AW-6026

DIN EN 573-3, DIN EN 754-2, DIN EN 754-3, DIN EN 755-2, DIN EN 755-3

EN AW-6082

Bar

EN AW-6082, EN AlSi1MgMn, EN AlMgSi1

DIN EN 573-3, DIN EN 754-2, DIN EN 754-4, DIN EN 755-2, DIN EN 755-4, DIN EN 515

EN CC483K

Bar

EN CC483K, EN CuSn12, DIN 2.1052, DIN GCuSn12

DIN EN 1982

EN CC493K

Bar, Tube

EN CC493K, EN CuSn7Zn4Pb7, DIN 2.1090, DIN GCuSn7ZnPb

DIN EN 1982

EN CC496K

Bar

EN CC496K, EN CuSn7Pb15, EN CuPb15Sn, DIN 2.1182, DIN GCuPb15Sn

DIN EN 1982

EN CuNi7Zn39Pb3Mn2

Bar

EN CW400J, EN CuNi7Zn39Pb3Mn2, DIN 2.0771, DIN CuNi7Zn39Pb3Mn2

DIN EN 12164