Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.4 g/cm³ Show Material materials with Dichte of 7.4 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 10 % Show Material materials with Dehnung of 10 % |
Härte, Brinell | 20.0 °C | 190 - 235 [-] Show Material materials with Härte, Brinell of 190 - 235 [-] |
Härte, Vickers | 20.0 °C | 200 - 245 [-] Show Material materials with Härte, Vickers of 200 - 245 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 MPa |
Zugfestigkeit | 20.0 °C | 750 MPa Show Material materials with Zugfestigkeit of 750 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 10.5 - 12.5 % Show Material materials with Aluminium of 10.5 - 12.5 % |
Andere | Rest Cu, total 0.2 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 5 - 7 % Show Material materials with Eisen of 5 - 7 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 5 - 7 % Show Material materials with Nickel of 5 - 7 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |