Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 5 % Show Material materials with Dehnung of 5 % |
Härte, Brinell | 20.0 °C | 130 [-] Show Material materials with Härte, Brinell of 130 [-] |
Härte, Vickers | 20.0 °C | 135 [-] Show Material materials with Härte, Vickers of 135 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 330 MPa Show Material materials with Streckgrenze Rp 0,2 of 330 MPa |
Zugfestigkeit | 20.0 °C | 480 MPa Show Material materials with Zugfestigkeit of 480 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.2 |
Blei | 1.6 - 3 % Show Material materials with Blei of 1.6 - 3 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 55 - 57 % Show Material materials with Kupfer of 55 - 57 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |