Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 12 % Show Material materials with Dehnung of 12 % |
Elastizitätsmodul | 20.0 °C | 108 GPa Show Material materials with Elastizitätsmodul of 108 GPa |
Härte, Brinell | 20.0 °C | 115 - 145 [-] Show Material materials with Härte, Brinell of 115 - 145 [-] |
Härte, Vickers | 20.0 °C | 120 - 150 [-] Show Material materials with Härte, Vickers of 120 - 150 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa |
Zugfestigkeit | 20.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.92E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.92E-5 1/K |
100.0 °C | 1.92E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.92E-5 1/K | |
Schmelzpunkt | 880 - 915 °C Show Material materials with Schmelzpunkt of 880 - 915 °C | |
Wärmeleitfähigkeit | 20.0 °C | 71 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 71 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 8.90E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 8.90E+6 S/m |
spezifischer Widerstand | 20.0 °C | 1.12E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.12E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.5 |
Blei | 0.8 % Show Material materials with Blei of 0.8 % |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % |
Kupfer | 66 - 70 % Show Material materials with Kupfer of 66 - 70 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Silizium | 0.7 - 1.3 % Show Material materials with Silizium of 0.7 - 1.3 % |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing : medium, soft brazing: medium | |
Workability | Cold forming degree between anneals: max. 80 %, general (condition): good |