spezifischer Widerstand: 1.12E-7 Ω·m

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Kohlenstoffarmer Stahl

EN 10277-2 Grade C15 cold drawn

Kohlenstoffarmer Stahl

DIN 1651 Grade 9SMn36 cold drawn

Kohlenstoffarmer Stahl

DIN 1651 Grade 9SMn36 untreated

Kohlenstoffarmer Stahl

ISO 683-4 Grade 11SMn37 untreated