Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 20 % Show Material materials with Dehnung of 20 % |
Härte, Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Härte, Brinell of 120 - 150 [-] |
Härte, Vickers | 20.0 °C | 125 - 155 [-] Show Material materials with Härte, Vickers of 125 - 155 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 300 MPa Show Material materials with Streckgrenze Rp 0,2 of 300 MPa |
Zugfestigkeit | 20.0 °C | 490 MPa Show Material materials with Zugfestigkeit of 490 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 1.3 % Show Material materials with Aluminium of 0.3 - 1.3 % |
Andere | Rest Zn, total 0.3 |
Blei | 0.2 - 0.8 % Show Material materials with Blei of 0.2 - 0.8 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 58 - 60 % Show Material materials with Kupfer of 58 - 60 % |
Mangan | 1.5 - 2.5 % Show Material materials with Mangan of 1.5 - 2.5 % |
Nickel | 2 - 3 % Show Material materials with Nickel of 2 - 3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |