Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.1 g/cm³ Show Material materials with Dichte of 8.1 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 15 % Show Material materials with Dehnung of 15 % |
Elastizitätsmodul | 23.0 °C | 93 GPa Show Material materials with Elastizitätsmodul of 93 GPa |
Härte, Brinell | 23.0 °C | 150 [-] Show Material materials with Härte, Brinell of 150 [-] |
Härte, Vickers | 23.0 °C | 150 [-] Show Material materials with Härte, Vickers of 150 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 280 MPa Show Material materials with Streckgrenze Rp 0,2 of 280 MPa |
Zugfestigkeit | 23.0 °C | 540 MPa Show Material materials with Zugfestigkeit of 540 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 2.04E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.04E-5 1/K |
100.0 °C | 2.04E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.04E-5 1/K | |
Schmelzpunkt | 865 - 885 °C Show Material materials with Schmelzpunkt of 865 - 885 °C | |
Wärmeleitfähigkeit | 23.0 °C | 63 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 63 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 7.80E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 7.80E+6 S/m |
spezifischer Widerstand | 23.0 °C | 1.28E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.28E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 1.3 - 2.3 % Show Material materials with Aluminium of 1.3 - 2.3 % |
Andere | Rest Zn, total 0.3 |
Blei | 0.2 - 0.8 % Show Material materials with Blei of 0.2 - 0.8 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kupfer | 57 - 59 % Show Material materials with Kupfer of 57 - 59 % |
Mangan | 1.5 - 3 % Show Material materials with Mangan of 1.5 - 3 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Silizium | 0.3 - 1.3 % Show Material materials with Silizium of 0.3 - 1.3 % |
Zinn | 0.4 % Show Material materials with Zinn of 0.4 % |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing : wenig geeignet, soft brazing: wenig geeignet | |
Workability | Cold forming degree between anneals: max. 15 %, general (condition): limited |