Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 18 % Show Material materials with Dehnung of 18 % |
Elastizitätsmodul | 20.0 °C | 93 GPa Show Material materials with Elastizitätsmodul of 93 GPa |
Härte, Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Härte, Brinell of 120 - 150 [-] |
Härte, Vickers | 20.0 °C | 125 - 155 [-] Show Material materials with Härte, Vickers of 125 - 155 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 210 MPa Show Material materials with Streckgrenze Rp 0,2 of 210 MPa |
Zugfestigkeit | 20.0 °C | 490 MPa Show Material materials with Zugfestigkeit of 490 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 2.11E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.11E-5 1/K |
100.0 °C | 2.11E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.11E-5 1/K | |
Schmelzpunkt | 860 - 910 °C Show Material materials with Schmelzpunkt of 860 - 910 °C | |
Wärmeleitfähigkeit | 20.0 °C | 80 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 80 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 7.80E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 7.80E+6 S/m |
spezifischer Widerstand | 20.0 °C | 1.28E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.28E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 1.3 % Show Material materials with Aluminium of 0.3 - 1.3 % |
Andere | Rest Zn, total 0.3 |
Blei | 1 % Show Material materials with Blei of 1 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kupfer | 59 - 61.5 % Show Material materials with Kupfer of 59 - 61.5 % |
Mangan | 0.6 - 1.8 % Show Material materials with Mangan of 0.6 - 1.8 % |
Nickel | 0.6 % Show Material materials with Nickel of 0.6 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |