AW Fraser produces and supplies, continuous cast and centrifugally cast bronze bars; hollow and solid brass extrusions; and, precision machined components from a variety of bronze and brass alloys.

Company profile

Headquarters

Christchurch, Canterbury, New Zealand

Type

Manufacturer and Processor

Certifications

ISO 14001

, ISO 9001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

Alloy LB2

Casting, Bar

UNS C93700, EN CC495K, DIN 2.1176, EN CuPb10Sn, JIS CAC603C, UNI 7013-72-3A

ASTM B505

Alloy LB4

Casting, Bar

UNS C93500, EN CC494K, EN CuSn5Pb9

ASTM B505

Alloy LG1

Casting, Bar

UNS C84400, EN CC490K, DIN 2.1098, EN CuSn2ZnPb, JIS CAC401

ASTM B505

Alloy LG2

Casting, Bar

UNS C83600, EN CC491K, DIN 2.0196, CuSn5ZnPb, JIS CAC402C, UNI 7013-72-8A

ASTM B271, ASTM B505

Alloy LG54

Casting, Bar

UNI 5275, UNS C95500, EN CC333G, DIN 2.0981, EN CuAl11Ni, JIS CAC703, BS AB2

ASTM B271, ASTM B505

Alloy PB1

Casting, Bar

UNS C90700, EN CC481K, DIN 2.1050, EN CuSn10, JIS CAC502C

ASTM B505

Alloy PB2

Casting, Bar

UNS C90800, EN CC483K, DIN 2.1052, CuSn12, JIS CAC502C, UNI 7013-72-2A

AS 1565

EN AcuZn34Al2

Casting, Bar

EN AcuZn34Al2

BS EN 1982

EN CuAl10Ni5Fe5

Casting, Bar

EN CuAl10Ni5Fe5, EN CC333G

BS EN 1982

UNS C35330

Casting, Bar

UNS C35330, EN CW602N, DIN 2.0371, EN CuZn36Pb3, BS CZ132

AS NZS 1567