Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 21 % Show Supplier Material materials with Dehnung of 21 % | min. | for thickness 5-150 mm | A8 | Transverse |
25 % Show Supplier Material materials with Dehnung of 25 % | min. | for thickness 5-150 mm | A2 | Transverse | |
Streckgrenze | 220 MPa Show Supplier Material materials with Streckgrenze of 220 MPa | min. | for thickness 5-150 mm | Transverse |
Zugfestigkeit | 415 - 550 MPa Show Supplier Material materials with Zugfestigkeit of 415 - 550 MPa | for thickness 5-150 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Kohlenstoff | 0.21 % Show Supplier Material materials with Kohlenstoff of 0.21 % | max. | for thickness 5-12.5 mm |
0.23 % Show Supplier Material materials with Kohlenstoff of 0.23 % | max. | for thickness 25-50 mm | |
0.25 % Show Supplier Material materials with Kohlenstoff of 0.25 % | max. | for thickness 50-80 mm | |
Mangan | 0.85 - 1.2 | for thickness 12.5-80 mm |
0.6 - 0.9 % Show Supplier Material materials with Mangan of 0.6 - 0.9 % | for thickness 5-12.5 mm | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. | for thickness 5-80 mm |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. | for thickness 5-80 mm |
Silizium | 0.15 - 0.4 % Show Supplier Material materials with Silizium of 0.15 - 0.4 % | for thickness 5-80 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Steel for pressure vessels are mainly used to manufacture boilers, drums, pressure or steam piping, industrial thermal vessels and heat exchangers. These steels are suitable for mechanical forming and welding. | |
Chemical composition | Manganese note: For each reduction by 0.01 percentage points below the specified maximum for carbon, an increase of 0.06 percentage points above the specified maximum for manganese is permitted, up to a maximum of 1.5% by heat analysis, and 1.6% by product analysis. | |
Delivery condtion | For the dimensions available please visit Dimension tables (see Table A). | |
Other | Available options Options available (after previous agreement): |