Kohlenstoffarmer Stahl
ASTM A612 As-Rolled or Normalized and/or Stress RelievedGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10250-2 Grade C25 normalized and tempered (+NT)Kohlenstoffarmer Stahl
EN 10250-2 Grade C25E normalized and tempered (+NT)Kohlenstoffarmer Stahl
EN 10250-2 Grade C25E quenched and tempered (+QT)Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Kohlenstoffarmer Stahl
EN 10083-1 Grade C25E quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10083-1 Grade C25R quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10083-2 Grade C25 quenched and tempered (+QT)Kohlenstoffarmer Stahl
BS 4360 Grade 43A Hot RolledMartensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT)Nickel-Kupfer-Legierung
DIN 17743 Grade NiCu30Fe soft annealed (+A)Kohlenstoffarmer Stahl
DIN 1681 Grade GS-38 heat treatedKohlenstoffarmer Stahl
DIN 1681 Grade GS-45 heat treated