Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | dry | ISO 1183 |
Sauerstoffindex | 38 % Show Supplier Material materials with Sauerstoffindex of 38 % | dry | ISO 4589-1/-2 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastizitätsmodul | 2.9 GPa Show Supplier Material materials with Elastizitätsmodul of 2.9 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 5.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5.5 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry | ISO 179/1eU |
Thermisch
Property | Value | Condition | Testing Standard | Pressure |
---|---|---|---|---|
Wärmeformbeständigkeitstemperatur | 139 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 139 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 2.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.5 [-] | dry | 1MHz | IEC 60250 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 6 cm³/10min | dry | ISO 1133 | 380°C/1kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts,Metal Tube Coating,Cable Ties,Chemical Process Industry,Chemical Process Industry - Coating of Chemical Pumps,Chemical Process Industry - Coating of Chemical Valves,Chemical Process Industry - Coating of Chemical Vessels,Chemical Process Industry - Injection Molding,Monofilaments,Packaging / Film,Powder Coatings - Wire Goods,Connectors E&E,Performance Wire,Wire and Cables,Natural Gas Distribution- Fittings | |
Processing methods | Injection Molding: |