Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.29 g/cm³ Show Supplier Material materials with Dichte of 1.29 g/cm³ | dry | ISO 1183 |
Sauerstoffindex | 35 % Show Supplier Material materials with Sauerstoffindex of 35 % | dry | ISO 4589-1/-2 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastizitätsmodul | 3.8 GPa Show Supplier Material materials with Elastizitätsmodul of 3.8 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 4.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.5 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 41 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 41 kJ/m² | dry | ISO 179/1eU |
23 °C | 62 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 62 kJ/m² | dry | ISO 179/1eU |
Thermisch
Property | Value | Condition | Testing Standard | Pressure |
---|---|---|---|---|
Wärmeformbeständigkeitstemperatur | 172 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 172 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 2.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.6 [-] | dry | 1MHz | IEC 60250 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 6 cm³/10min | dry | ISO 1133 | 380°C/1kg |
Technological properties
Property | ||
---|---|---|
Processing methods | Injection Molding: |