Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.52 g/cm³ Show Supplier Material materials with Dichte of 1.52 g/cm³ | dry | ISO 1183 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 7 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 7 cm³/10min | dry | ISO 1133 | 380°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Connectors E&E | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding: |