Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Kynar 500® FSF®
Kynar 500® FSF® PVDF resin is used by leading coating formulators as a base vehicle in long-life coatings for aluminum, galvanized steel and aluminized steel.
Today,
Kynar 500® FSF® PVDF resin-based metal coatings provide billions of square feet of protection against weathering, aging and pollution on commercial, industrial, institutional and residential buildings around the globe. The capability of Kynar 500® resins to deliver long-term durability is unparalleled in the industry. Introduced in 1965, Kynar 500® resin-based coatings were the original high performance finishes for architectural metal. According to a recent survey, Kynar 500® finishes are still the architect’s first choice.
Diese Materialdaten wurden von Arkema Technical Polymers zur Verfügung gestellt
All categories
Mechanisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Streckgrenze | 21 MPa Show Supplier Material materials with Streckgrenze of 21 MPa | dry | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Application areas | Factory Applied |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.