Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Coefficient of friction | 0.54 [-] Show Supplier Material materials with Coefficient of friction of 0.54 [-] | ASTM D1894 | vs Steel, Kinetic | |
0.55 [-] Show Supplier Material materials with Coefficient of friction of 0.55 [-] | ASTM D1894 | vs Steel, Static | ||
Dichte | 1.78 - 1.8 g/cm³ Show Supplier Material materials with Dichte of 1.78 - 1.8 g/cm³ | ASTM D792 | ||
1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | ISO 1183 | dry | ||
Sauerstoffindex | 43 % Show Supplier Material materials with Sauerstoffindex of 43 % | ASTM D2863 | ||
49 % Show Supplier Material materials with Sauerstoffindex of 49 % | ISO 4589-1/-2 | dry | ||
Wasserabsorption | 0.03 % Show Supplier Material materials with Wasserabsorption of 0.03 % | Sim. to ISO 62 | ||
0.03 - 0.06 % Show Supplier Material materials with Wasserabsorption of 0.03 - 0.06 % | ASTM D570 |
Mechanisch
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Biegefestigkeit | 13.8 - 24.1 MPa Show Supplier Material materials with Biegefestigkeit of 13.8 - 24.1 MPa | ASTM D790 | at 5% strain | |
Biegemodul | 0.276 - 0.414 GPa Show Supplier Material materials with Biegemodul of 0.276 - 0.414 GPa | ASTM D790 | ||
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527-1/-2 | dry | min. | nominal |
200 - 400 % Show Supplier Material materials with Dehnung of 200 - 400 % | ASTM D638 | |||
Druckfestigkeit | 24.1 - 31 MPa Show Supplier Material materials with Druckfestigkeit of 24.1 - 31 MPa | ASTM D695 | ||
Elastizitätsmodul | 0.276 - 0.448 GPa Show Supplier Material materials with Elastizitätsmodul of 0.276 - 0.448 GPa | ASTM D638 | ||
0.526 GPa Show Supplier Material materials with Elastizitätsmodul of 0.526 GPa | ISO 527-1/-2 | dry | ||
Elongation at yield | 15 - 25 % Show Supplier Material materials with Elongation at yield of 15 - 25 % | ASTM D638 | ||
15 % Show Supplier Material materials with Elongation at yield of 15 % | ISO 527-1/-2 | dry | ||
Härte, Shore D | 57 - 62 [-] Show Supplier Material materials with Härte, Shore D of 57 - 62 [-] | ASTM D2240 | ||
Schlagfestigkeit, Charpy gekerbt | No Break at 23°C | ISO 179/1eA | dry | |
Streckgrenze | 13.8 - 21.4 MPa Show Supplier Material materials with Streckgrenze of 13.8 - 21.4 MPa | ASTM D638 | ||
27 MPa Show Supplier Material materials with Streckgrenze of 27 MPa | ISO 527-1/-2 | dry | ||
Zugfestigkeit | 20 - 27.6 MPa Show Supplier Material materials with Zugfestigkeit of 20 - 27.6 MPa | ASTM D638 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | dry | ASTM D7028, ISO 11357-1/-2 | 10°C/min | |||||
Koeffizient der thermischen Ausdehnung | 0.000162 - 0.000216 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000162 - 0.000216 1/K | ASTM D696 | |||||||
0.000177 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000177 1/K | dry | ISO 11359-1/-2 | |||||||
Schmelzpunkt | 130 - 138 °C Show Supplier Material materials with Schmelzpunkt of 130 - 138 °C | ASTM D3418 | |||||||
134 °C Show Supplier Material materials with Schmelzpunkt of 134 °C | dry | ISO 11357-1/-3 | 10°C/min | ||||||
Spezifische Wärmekapazität | 745 - 958 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 745 - 958 J/(kg·K) | DSC | |||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Vicat-Erweichungstemperatur | 61 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 61 °C | ISO 306 | 50°C/h 50N | ||||||
Wärmeformbeständigkeitstemperatur | 35 - 52 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 35 - 52 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
43 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 43 °C | dry | ISO 75-1/-2 | 2 MPa | ||||||
49 - 66 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 49 - 66 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
57 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 57 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||||||
Wärmeleitfähigkeit | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Entflammbarkeit | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Elektrisch
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Dielektrizitätskonstante | 3.8 - 12.1 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 - 12.1 [-] | 1KHz | ASTM D150 | |
7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7 [-] | 1MHz | IEC 60250 | dry | |
11.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 11.5 [-] | 100Hz | IEC 60250 | dry | |
Durchschlagfestigkeit | 43.3 - 51.2 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 43.3 - 51.2 kV/mm | ASTM D149 | ||
Surface resistivity | 4.8e+11 - 5.1e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 4.8e+11 - 5.1e+11 Ω/sq | ASTM D257 | ||
Verlustfaktor | 0.02 - 0.24 [-] Show Supplier Material materials with Verlustfaktor of 0.02 - 0.24 [-] | 100KHz | ASTM D150 | |
0.024 [-] Show Supplier Material materials with Verlustfaktor of 0.024 [-] | 100Hz | IEC 60250 | dry | |
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH | |
2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | IEC 60093 | dry |
Optisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Brechungsindex | 1 [-] Show Supplier Material materials with Brechungsindex of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 2000 - 2500 Pa·s Show Supplier Material materials with Melt viscosity of 2000 - 2500 Pa·s | ASTM D3835 | ||
Schmelzmassenflussrate | 4 - 14 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 4 - 14 g/10min | ASTM D1238 | 230°C/12.5kg | |
Schmelzvolumenflussrate | 1.9 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 1.9 cm³/10min | ISO 1133 | dry | 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines,Chemical Process Industry,Tubing and Hoses,Performance Wire,Offshore Umbilicals | |
Processing methods | Injection Molding: |