Allgemein
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Coefficient of friction | 0.33 [-] Show Supplier Material materials with Coefficient of friction of 0.33 [-] | ASTM D1894 | vs Steel, Static | |
0.33 [-] Show Supplier Material materials with Coefficient of friction of 0.33 [-] | ASTM D1894 | vs Steel, Kinetic | ||
Dichte | 1.77 - 1.8 g/cm³ Show Supplier Material materials with Dichte of 1.77 - 1.8 g/cm³ | ASTM D792 | ||
1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | ISO 1183 | dry | ||
Moisture absorption | 0.015 % Show Supplier Material materials with Moisture absorption of 0.015 % | Sim. to ISO 62 | ||
Sauerstoffindex | 42 % Show Supplier Material materials with Sauerstoffindex of 42 % | ASTM D2863 | ||
43 % Show Supplier Material materials with Sauerstoffindex of 43 % | ISO 4589-1/-2 | dry | ||
Wasserabsorption | 0.03 % Show Supplier Material materials with Wasserabsorption of 0.03 % | Sim. to ISO 62 | ||
0.03 - 0.05 % Show Supplier Material materials with Wasserabsorption of 0.03 - 0.05 % | ASTM D570 |
Mechanisch
Property | Temperature | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 20.7 - 34.5 MPa Show Supplier Material materials with Biegefestigkeit of 20.7 - 34.5 MPa | ASTM D790 | at 5% strain | ||
Biegemodul | 0.483 - 0.758 GPa Show Supplier Material materials with Biegemodul of 0.483 - 0.758 GPa | ASTM D790 | |||
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527-1/-2 | dry | min. | nominal | |
100 - 300 % Show Supplier Material materials with Dehnung of 100 - 300 % | ASTM D638 | ||||
Druckfestigkeit | 31 - 41.4 MPa Show Supplier Material materials with Druckfestigkeit of 31 - 41.4 MPa | ASTM D695 | |||
Elastizitätsmodul | 0.552 - 0.896 GPa Show Supplier Material materials with Elastizitätsmodul of 0.552 - 0.896 GPa | ASTM D638 | |||
0.7 GPa Show Supplier Material materials with Elastizitätsmodul of 0.7 GPa | ISO 527-1/-2 | dry | |||
Elongation at yield | 10 - 20 % Show Supplier Material materials with Elongation at yield of 10 - 20 % | ASTM D638 | |||
15 % Show Supplier Material materials with Elongation at yield of 15 % | ISO 527-1/-2 | dry | |||
Härte, Shore D | 60 - 70 [-] Show Supplier Material materials with Härte, Shore D of 60 - 70 [-] | ASTM D2240 | |||
Impact strength, Charpy notched, ASTM | 23 °C | 534 - 1070 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 534 - 1070 J/m | ASTM D256 | ||
Impact strength, Charpy unnotched, ASTM | No Break at 23°C | ASTM D256 | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179/1eA | dry | No Break at 23°C |
Streckgrenze | 20 - 34.5 MPa Show Supplier Material materials with Streckgrenze of 20 - 34.5 MPa | ASTM D638 | |||
27 MPa Show Supplier Material materials with Streckgrenze of 27 MPa | ISO 527-1/-2 | dry | |||
Zugfestigkeit | 17.2 - 34.5 MPa Show Supplier Material materials with Zugfestigkeit of 17.2 - 34.5 MPa | ASTM D638 |
Thermisch
Property | Value | Testing Standard | Condition | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -41.1 - -39.4 °C Show Supplier Material materials with Glasübergangstemperatur of -41.1 - -39.4 °C | ASTM D7028 | |||||||
-40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | ISO 11357-1/-2 | dry | 10°C/min | ||||||
Koeffizient der thermischen Ausdehnung | 0.000126 - 0.000185 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000126 - 0.000185 1/K | ASTM D696 | |||||||
0.00016 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00016 1/K | ISO 11359-1/-2 | dry | |||||||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||||||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||||||
Schmelzpunkt | 140 - 145 °C Show Supplier Material materials with Schmelzpunkt of 140 - 145 °C | ASTM D3418 | |||||||
143 °C Show Supplier Material materials with Schmelzpunkt of 143 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Spezifische Wärmekapazität | 745 - 958 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 745 - 958 J/(kg·K) | DSC | |||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Vicat-Erweichungstemperatur | 79 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 79 °C | ISO 306 | 50°C/h 50N | ||||||
Wärmeformbeständigkeitstemperatur | 40 - 55 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 40 - 55 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
48 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 48 °C | ISO 75-1/-2 | dry | 2 MPa | ||||||
60 - 75 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 60 - 75 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
68 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 68 °C | ISO 75-1/-2 | dry | 0.45 MPa | ||||||
Wärmeleitfähigkeit | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Entflammbarkeit | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available |
Elektrisch
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Dielektrizitätskonstante | 3.5 - 10.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 - 10.6 [-] | 1KHz | ASTM D150 | |
7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7 [-] | 1MHz | IEC 60250 | dry | |
11 [-] Show Supplier Material materials with Dielektrizitätskonstante of 11 [-] | 100Hz | IEC 60250 | dry | |
Durchschlagfestigkeit | 51.2 - 59.1 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 51.2 - 59.1 kV/mm | ASTM D149 | ||
Surface resistivity | 5.1e+11 - 5.3e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 5.1e+11 - 5.3e+11 Ω/sq | ASTM D257 | ||
Verlustfaktor | 0.02 - 0.21 [-] Show Supplier Material materials with Verlustfaktor of 0.02 - 0.21 [-] | 100KHz | ASTM D150 | |
0.052 [-] Show Supplier Material materials with Verlustfaktor of 0.052 [-] | 100Hz | IEC 60250 | dry | |
0.233 [-] Show Supplier Material materials with Verlustfaktor of 0.233 [-] | 1MHz | IEC 60250 | dry | |
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH | |
2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | IEC 60093 | dry |
Optisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Brechungsindex | 1 [-] Show Supplier Material materials with Brechungsindex of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 2700 - 220000 Pa·s Show Supplier Material materials with Melt viscosity of 2700 - 220000 Pa·s | ASTM D3835 | ||
Schmelzmassenflussrate | 3 - 8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 3 - 8 g/10min | ASTM D1238 | 230°C/12.5kg | |
Schmelzvolumenflussrate | 0.5 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 0.5 cm³/10min | ISO 1133 | dry | 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Tubing and Hoses,Automotive Cables,Performance Wire,PVDF Cable Jacketing,Wire and Cables,Offshore Umbilicals,Underground Fuel Containment | |
Processing methods | Compression Molding: |