Das Material: 'Kynar Flex® 2800-00', nach dem Sie gesucht haben, wurde durch das untenstehende ersetzt.

Kynar Flex® 2800-00

Alternative und Handelsbezeichungen
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

Kynar Flex® 2800-00 resin is a standard grade of granules, compared to the homopolymer grades, which exhibits a lower modulus, a better resistance to stress cracking in alkaline and oxidizing media, and a lower melting point. For cable coating, extrusion of tube and plaque, compression molding of bulky parts.

Additional characteristics:

  • Easily processed using conventional equipment
  • Excellent thermal stability
  • Retains properties after aging
  • Pigmentable
  • UL RTI temperature rating 125ºC
  • Radiation crosslinking

  • Diese Materialdaten wurden von Arkema Technical Polymers zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Eigenschaften

    Allgemein

    PropertyValueTesting StandardConditionComment

    Coefficient of friction

    0.33 [-]

    Show Supplier Material materials with Coefficient of friction of 0.33 [-]

    ASTM D1894

    vs Steel, Static

    0.33 [-]

    Show Supplier Material materials with Coefficient of friction of 0.33 [-]

    ASTM D1894

    vs Steel, Kinetic

    Dichte

    1.77 - 1.8 g/cm³

    Show Supplier Material materials with Dichte of 1.77 - 1.8 g/cm³

    ASTM D792

    1.78 g/cm³

    Show Supplier Material materials with Dichte of 1.78 g/cm³

    ISO 1183

    dry

    Moisture absorption

    0.015 %

    Show Supplier Material materials with Moisture absorption of 0.015 %

    Sim. to ISO 62

    Sauerstoffindex

    42 %

    Show Supplier Material materials with Sauerstoffindex of 42 %

    ASTM D2863

    43 %

    Show Supplier Material materials with Sauerstoffindex of 43 %

    ISO 4589-1/-2

    dry

    Wasserabsorption

    0.03 %

    Show Supplier Material materials with Wasserabsorption of 0.03 %

    Sim. to ISO 62

    0.03 - 0.05 %

    Show Supplier Material materials with Wasserabsorption of 0.03 - 0.05 %

    ASTM D570

    Mechanisch

    PropertyTemperatureValueTesting StandardConditionComment

    Biegefestigkeit

    20.7 - 34.5 MPa

    Show Supplier Material materials with Biegefestigkeit of 20.7 - 34.5 MPa

    ASTM D790

    at 5% strain

    Biegemodul

    0.483 - 0.758 GPa

    Show Supplier Material materials with Biegemodul of 0.483 - 0.758 GPa

    ASTM D790

    Dehnung

    50 %

    Show Supplier Material materials with Dehnung of 50 %

    ISO 527-1/-2

    dry

    min. | nominal

    100 - 300 %

    Show Supplier Material materials with Dehnung of 100 - 300 %

    ASTM D638

    Druckfestigkeit

    31 - 41.4 MPa

    Show Supplier Material materials with Druckfestigkeit of 31 - 41.4 MPa

    ASTM D695

    Elastizitätsmodul

    0.552 - 0.896 GPa

    Show Supplier Material materials with Elastizitätsmodul of 0.552 - 0.896 GPa

    ASTM D638

    0.7 GPa

    Show Supplier Material materials with Elastizitätsmodul of 0.7 GPa

    ISO 527-1/-2

    dry

    Elongation at yield

    10 - 20 %

    Show Supplier Material materials with Elongation at yield of 10 - 20 %

    ASTM D638

    15 %

    Show Supplier Material materials with Elongation at yield of 15 %

    ISO 527-1/-2

    dry

    Härte, Shore D

    60 - 70 [-]

    Show Supplier Material materials with Härte, Shore D of 60 - 70 [-]

    ASTM D2240

    Impact strength, Charpy notched, ASTM

    23 °C

    534 - 1070 J/m

    Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 534 - 1070 J/m

    ASTM D256

    Impact strength, Charpy unnotched, ASTM

    No Break at 23°C

    ASTM D256

    Schlagfestigkeit, Charpy gekerbt

    -30 °C

    5 kJ/m²

    Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m²

    ISO 179/1eA

    dry

    No Break at 23°C

    Streckgrenze

    20 - 34.5 MPa

    Show Supplier Material materials with Streckgrenze of 20 - 34.5 MPa

    ASTM D638

    27 MPa

    Show Supplier Material materials with Streckgrenze of 27 MPa

    ISO 527-1/-2

    dry

    Zugfestigkeit

    17.2 - 34.5 MPa

    Show Supplier Material materials with Zugfestigkeit of 17.2 - 34.5 MPa

    ASTM D638

    Thermisch

    PropertyValueTesting StandardConditionPressureComment

    Glasübergangstemperatur

    -41.1 - -39.4 °C

    Show Supplier Material materials with Glasübergangstemperatur of -41.1 - -39.4 °C

    ASTM D7028

    -40 °C

    Show Supplier Material materials with Glasübergangstemperatur of -40 °C

    ISO 11357-1/-2

    dry

    10°C/min

    Koeffizient der thermischen Ausdehnung

    0.000126 - 0.000185 1/K

    Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000126 - 0.000185 1/K

    ASTM D696

    0.00016 1/K

    Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00016 1/K

    ISO 11359-1/-2

    dry

    Relative temperature index, electrical

    130 °C

    Show Supplier Material materials with Relative temperature index, electrical of 130 °C

    UL 746B

    Relative temperature index, mechanical strength

    130 °C

    Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C

    UL 746B

    Schmelzpunkt

    140 - 145 °C

    Show Supplier Material materials with Schmelzpunkt of 140 - 145 °C

    ASTM D3418

    143 °C

    Show Supplier Material materials with Schmelzpunkt of 143 °C

    ISO 11357-1/-3

    dry

    10°C/min

    Spezifische Wärmekapazität

    745 - 958 J/(kg·K)

    Show Supplier Material materials with Spezifische Wärmekapazität of 745 - 958 J/(kg·K)

    DSC

    Thermal decomposition in air

    375 °C

    Show Supplier Material materials with Thermal decomposition in air of 375 °C

    TGA

    1% wt. loss

    Thermal decomposition in nitrogen

    410 °C

    Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

    TGA

    1% wt. loss

    Vicat-Erweichungstemperatur

    79 °C

    Show Supplier Material materials with Vicat-Erweichungstemperatur of 79 °C

    ISO 306

    50°C/h 50N

    Wärmeformbeständigkeitstemperatur

    40 - 55 °C

    Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 40 - 55 °C

    ASTM D648

    2 MPa

    248 °F/hr

    48 °C

    Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 48 °C

    ISO 75-1/-2

    dry

    2 MPa

    60 - 75 °C

    Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 60 - 75 °C

    ASTM D648

    0.45 MPa

    248 °F/hr

    68 °C

    Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 68 °C

    ISO 75-1/-2

    dry

    0.45 MPa

    Wärmeleitfähigkeit

    0.144 - 0.18 W/(m·K)

    Show Supplier Material materials with Wärmeleitfähigkeit of 0.144 - 0.18 W/(m·K)

    ASTM D433

    Entflammbarkeit

    At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available

    Elektrisch

    PropertyValueFrequencyTesting StandardCondition

    Dielektrizitätskonstante

    3.5 - 10.6 [-]

    Show Supplier Material materials with Dielektrizitätskonstante of 3.5 - 10.6 [-]

    1KHz

    ASTM D150

    7 [-]

    Show Supplier Material materials with Dielektrizitätskonstante of 7 [-]

    1MHz

    IEC 60250

    dry

    11 [-]

    Show Supplier Material materials with Dielektrizitätskonstante of 11 [-]

    100Hz

    IEC 60250

    dry

    Durchschlagfestigkeit

    51.2 - 59.1 kV/mm

    Show Supplier Material materials with Durchschlagfestigkeit of 51.2 - 59.1 kV/mm

    ASTM D149

    Surface resistivity

    5.1e+11 - 5.3e+11 Ω/sq

    Show Supplier Material materials with Surface resistivity of 5.1e+11 - 5.3e+11 Ω/sq

    ASTM D257

    Verlustfaktor

    0.02 - 0.21 [-]

    Show Supplier Material materials with Verlustfaktor of 0.02 - 0.21 [-]

    100KHz

    ASTM D150

    0.052 [-]

    Show Supplier Material materials with Verlustfaktor of 0.052 [-]

    100Hz

    IEC 60250

    dry

    0.233 [-]

    Show Supplier Material materials with Verlustfaktor of 0.233 [-]

    1MHz

    IEC 60250

    dry

    Volume resistivity

    2e+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

    ASTM D257

    65% RH

    2e+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

    IEC 60093

    dry

    Optisch

    PropertyValueTesting StandardComment

    Brechungsindex

    1 [-]

    Show Supplier Material materials with Brechungsindex of 1 [-]

    ASTM D542

    sodium D line

    Rheological Properties

    PropertyValueTesting StandardConditionComment

    Melt viscosity

    2700 - 220000 Pa·s

    Show Supplier Material materials with Melt viscosity of 2700 - 220000 Pa·s

    ASTM D3835

    Schmelzmassenflussrate

    3 - 8 g/10min

    Show Supplier Material materials with Schmelzmassenflussrate of 3 - 8 g/10min

    ASTM D1238

    230°C/12.5kg

    Schmelzvolumenflussrate

    0.5 cm³/10min

    Show Supplier Material materials with Schmelzvolumenflussrate of 0.5 cm³/10min

    ISO 1133

    dry

    230°C/5kg

    Technological properties

    Property
    Application areas

    Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Tubing and Hoses,Automotive Cables,Performance Wire,PVDF Cable Jacketing,Wire and Cables,Offshore Umbilicals,Underground Fuel Containment

    Processing methods

    Compression Molding:

  • Molding temperature (°C) ISO 293: 225
  • Molding time (min) ISO 293: 3
  • DeMolding temperature (°C) ISO 293: 120