Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.77 - 1.8 g/cm³ Show Supplier Material materials with Dichte of 1.77 - 1.8 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Biegefestigkeit | 20.7 - 34.5 MPa Show Supplier Material materials with Biegefestigkeit of 20.7 - 34.5 MPa | ASTM D790 | at 5% strain | |
Biegemodul | 1.0 - 1.2 GPa Show Supplier Material materials with Biegemodul of 1.0 - 1.2 GPa | ASTM D790 | ||
Dehnung | 30 - 200 % Show Supplier Material materials with Dehnung of 30 - 200 % | ASTM D638 | ||
Druckfestigkeit | 41.4 - 58.6 MPa Show Supplier Material materials with Druckfestigkeit of 41.4 - 58.6 MPa | ASTM D695 | ||
Härte, Shore D | 70 - 75 [-] Show Supplier Material materials with Härte, Shore D of 70 - 75 [-] | ASTM D2240 | ||
Streckgrenze | 31 - 41.4 MPa Show Supplier Material materials with Streckgrenze of 31 - 41.4 MPa | ASTM D638 | ||
40 MPa Show Supplier Material materials with Streckgrenze of 40 MPa | ISO 527-1/-2 | dry | ||
Zugfestigkeit | 27.6 - 48.3 MPa Show Supplier Material materials with Zugfestigkeit of 27.6 - 48.3 MPa | ASTM D638 |
Thermisch
Property | Value | Testing Standard |
---|---|---|
Schmelzpunkt | 155 - 160 °C Show Supplier Material materials with Schmelzpunkt of 155 - 160 °C | ASTM D3418 |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | 65% RH | ASTM D257 |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 2300 - 2700 Pa·s Show Supplier Material materials with Melt viscosity of 2300 - 2700 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Plenum Pipe,Wire and Cables |