Allgemein
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Coefficient of friction | 0.54 [-] Show Supplier Material materials with Coefficient of friction of 0.54 [-] | ASTM D1894 | vs Steel, Kinetic | |
0.55 [-] Show Supplier Material materials with Coefficient of friction of 0.55 [-] | ASTM D1894 | vs Steel, Static | ||
Dichte | 1.77 - 1.8 g/cm³ Show Supplier Material materials with Dichte of 1.77 - 1.8 g/cm³ | ASTM D792 | ||
1.77 g/cm³ Show Supplier Material materials with Dichte of 1.77 g/cm³ | ISO 1183 | dry | ||
Sauerstoffindex | 95 % Show Supplier Material materials with Sauerstoffindex of 95 % | ASTM D2863, ISO 4589-1/-2 | dry | |
Wasserabsorption | 0.03 % Show Supplier Material materials with Wasserabsorption of 0.03 % | Sim. to ISO 62 | ||
0.03 - 0.05 % Show Supplier Material materials with Wasserabsorption of 0.03 - 0.05 % | ASTM D570 |
Mechanisch
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Biegefestigkeit | 13.8 - 24.1 MPa Show Supplier Material materials with Biegefestigkeit of 13.8 - 24.1 MPa | ASTM D790 | at 5% strain | |
Biegemodul | 0.276 - 0.414 GPa Show Supplier Material materials with Biegemodul of 0.276 - 0.414 GPa | ASTM D790 | ||
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527-1/-2 | dry | min. | nominal |
200 - 400 % Show Supplier Material materials with Dehnung of 200 - 400 % | ASTM D638 | |||
Druckfestigkeit | 24.1 - 31 MPa Show Supplier Material materials with Druckfestigkeit of 24.1 - 31 MPa | ASTM D695 | ||
Elastizitätsmodul | 0.276 - 0.448 GPa Show Supplier Material materials with Elastizitätsmodul of 0.276 - 0.448 GPa | ASTM D638 | ||
0.387 GPa Show Supplier Material materials with Elastizitätsmodul of 0.387 GPa | ISO 527-1/-2 | dry | ||
Elongation at yield | 15 - 25 % Show Supplier Material materials with Elongation at yield of 15 - 25 % | ASTM D638 | ||
18 % Show Supplier Material materials with Elongation at yield of 18 % | ISO 527-1/-2 | dry | ||
Härte, Shore D | 57 - 62 [-] Show Supplier Material materials with Härte, Shore D of 57 - 62 [-] | ASTM D2240 | ||
Impact strength, Charpy notched, ASTM | No Break at 23°C | ASTM D256 | ||
Impact strength, Charpy unnotched, ASTM | No Break at 23°C | ASTM D256 | ||
Schlagfestigkeit, Charpy gekerbt | No Break at 23°C | ISO 179/1eA | dry | |
Streckgrenze | 12 MPa Show Supplier Material materials with Streckgrenze of 12 MPa | ISO 527-1/-2 | dry | |
13.8 - 21.4 MPa Show Supplier Material materials with Streckgrenze of 13.8 - 21.4 MPa | ASTM D638 | |||
Zugfestigkeit | 20 - 27.6 MPa Show Supplier Material materials with Zugfestigkeit of 20 - 27.6 MPa | ASTM D638 |
Thermisch
Property | Value | Testing Standard | Condition | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -42.2 - -40 °C Show Supplier Material materials with Glasübergangstemperatur of -42.2 - -40 °C | ASTM D7028 | |||||||
-40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | ISO 11357-1/-2 | dry | 10°C/min | ||||||
Koeffizient der thermischen Ausdehnung | 0.000162 - 0.000216 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000162 - 0.000216 1/K | ASTM D696 | |||||||
Schmelzpunkt | 130 - 138 °C Show Supplier Material materials with Schmelzpunkt of 130 - 138 °C | ASTM D3418 | |||||||
134 °C Show Supplier Material materials with Schmelzpunkt of 134 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Spezifische Wärmekapazität | 745 - 958 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 745 - 958 J/(kg·K) | DSC | |||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Wärmeformbeständigkeitstemperatur | 35 - 52 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 35 - 52 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
43 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 43 °C | ISO 75-1/-2 | dry | 2 MPa | ||||||
49 - 66 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 49 - 66 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
57 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 57 °C | ISO 75-1/-2 | dry | 0.45 MPa | ||||||
Wärmeleitfähigkeit | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Entflammbarkeit | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available |
Elektrisch
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Dielektrizitätskonstante | 3.8 - 12.1 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 - 12.1 [-] | 1KHz | ASTM D150 | |
7.05 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7.05 [-] | 100Hz | IEC 60250 | dry | |
Durchschlagfestigkeit | 1.4 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 1.4 kV/mm | IEC 60243-1 | dry | |
43.3 - 51.2 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 43.3 - 51.2 kV/mm | ASTM D149 | |||
Verlustfaktor | 1.2e-05 [-] Show Supplier Material materials with Verlustfaktor of 1.2e-05 [-] | 100Hz | IEC 60250 | dry |
0.02 - 0.24 [-] Show Supplier Material materials with Verlustfaktor of 0.02 - 0.24 [-] | 100KHz | ASTM D150 | ||
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH | |
2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | IEC 60093 | dry |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 6 - 1200 Pa·s Show Supplier Material materials with Melt viscosity of 6 - 1200 Pa·s | ASTM D3835 | ||
Schmelzmassenflussrate | 8 - 25 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 8 - 25 g/10min | ASTM D1238 | 230°C/3.8kg | |
Schmelzvolumenflussrate | 11.5 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 11.5 cm³/10min | ISO 1133 | dry | 232°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Cables,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables |