Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.78 - 1.82 g/cm³ Show Supplier Material materials with Dichte of 1.78 - 1.82 g/cm³ | ASTM D792 | |
Sauerstoffindex | 43 % Show Supplier Material materials with Sauerstoffindex of 43 % | ASTM D2863 | |
Wasserabsorption | 0.5 % Show Supplier Material materials with Wasserabsorption of 0.5 % | ASTM D570 | max. |
Mechanisch
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Biegemodul | 0.248 - 0.303 GPa Show Supplier Material materials with Biegemodul of 0.248 - 0.303 GPa | ASTM D790 | ||
Dehnung | 500 % Show Supplier Material materials with Dehnung of 500 % | ASTM D638 | min. | |
Elastizitätsmodul | 0.207 - 0.345 GPa Show Supplier Material materials with Elastizitätsmodul of 0.207 - 0.345 GPa | ASTM D638 | ||
Elongation at yield | 25 - 40 % Show Supplier Material materials with Elongation at yield of 25 - 40 % | ASTM D638 | ||
Härte, Shore D | 50 - 60 [-] Show Supplier Material materials with Härte, Shore D of 50 - 60 [-] | ASTM D2240 | ||
Impact strength, Charpy notched, ASTM | No Break at 23°C | ASTM D256 | ||
Streckgrenze | 11.7 - 15.9 MPa Show Supplier Material materials with Streckgrenze of 11.7 - 15.9 MPa | ASTM D638 | ||
27 MPa Show Supplier Material materials with Streckgrenze of 27 MPa | ISO 527-1/-2 | dry | ||
Zugfestigkeit | 18.6 - 24.1 MPa Show Supplier Material materials with Zugfestigkeit of 18.6 - 24.1 MPa | ASTM D638 |
Thermisch
Property | Value | Testing Standard |
---|---|---|
Glasübergangstemperatur | -40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | ASTM D7028 |
Koeffizient der thermischen Ausdehnung | 0.000153 - 0.000194 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000153 - 0.000194 1/K | ASTM D696 |
Schmelzpunkt | 160 - 168 °C Show Supplier Material materials with Schmelzpunkt of 160 - 168 °C | ASTM D3418 |
Elektrisch
Property | Value | Testing Standard | Condition |
---|---|---|---|
Durchschlagfestigkeit | 39.4 - 47.2 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 39.4 - 47.2 kV/mm | ASTM D149 | |
Surface resistivity | 7.6e+11 - 7.9e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 7.6e+11 - 7.9e+11 Ω/sq | ASTM D257 | |
Volume resistivity | 7.8e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 7.8e+13 Ω·cm | ||
8e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 8e+13 Ω·cm | ASTM D257 | 65% RH |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt viscosity | 2100 - 2600 Pa·s Show Supplier Material materials with Melt viscosity of 2100 - 2600 Pa·s | ASTM D3835 | |
Schmelzmassenflussrate | 2.5 - 7.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 2.5 - 7.5 g/10min | ASTM D1238 | 230°C/12.5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Auto - Water Cooling Circuit,Automotive Cables,Foamed PVDF Cable Jacketing,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables |