Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.79 g/cm³ Show Supplier Material materials with Dichte of 1.79 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | Sim. to ISO 62 |
Mechanisch
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 13 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 13 kV/mm | dry | IEC 60243-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 6 cm³/10min | dry | ISO 1133 | 230°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Potable Water Distribution |