Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | dry | ISO 1183, ASTM D792 | min. |
Wasserabsorption | 0.03 % Show Supplier Material materials with Wasserabsorption of 0.03 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Biegemodul | 1.0 GPa Show Supplier Material materials with Biegemodul of 1.0 GPa | ASTM D790 | ||
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527-1/-2 | dry | min. | nominal |
400 % Show Supplier Material materials with Dehnung of 400 % | ASTM D638 | min. | ||
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | ISO 527-1/-2 | dry | |
Schlagfestigkeit, Charpy gekerbt | No Break at 23°C | ISO 179/1eA | dry | |
Streckgrenze | 35 MPa Show Supplier Material materials with Streckgrenze of 35 MPa | ASTM D638 |
Thermisch
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Schmelzpunkt | 151 - 157 °C Show Supplier Material materials with Schmelzpunkt of 151 - 157 °C | ASTM D3418 | ||
154 °C Show Supplier Material materials with Schmelzpunkt of 154 °C | ISO 11357-1/-3 | dry | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 3400 - 3800 Pa·s Show Supplier Material materials with Melt viscosity of 3400 - 3800 Pa·s | ASTM D3835 | ||
Schmelzmassenflussrate | 3 - 8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 3 - 8 g/10min | ASTM D1238 | 230°C/21.6kg | |
Schmelzvolumenflussrate | 3.2 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 3.2 cm³/10min | ISO 1133 | dry | 232°C/21.6kg |
Technological properties
Property | ||
---|---|---|
Application areas | Lithium Ion Battery Binder,Lithium ion Battery Separator Coating |