Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Kynar Flex® LBG2200LX
Kynar Flex® LBG2200LX is a lithium ion battery grade latex of vinylidene fluoride and hexafluoropropylene designed for high performance.
Main Characteristics:
Diese Materialdaten wurden von Arkema Technical Polymers zur Verfügung gestellt
All categories
Thermisch
Property | Value | Testing Standard |
---|---|---|
Schmelzpunkt | 148 - 154 °C Show Supplier Material materials with Schmelzpunkt of 148 - 154 °C | ASTM D3418 |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 3200 - 3700 Pa·s Show Supplier Material materials with Melt viscosity of 3200 - 3700 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Lithium Ion Battery Binder,Lithium ion Battery Separator Coating |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.