Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | ASTM D792 | min. |
Thermisch
Property | Value | Testing Standard |
---|---|---|
Schmelzpunkt | 142 - 148 °C Show Supplier Material materials with Schmelzpunkt of 142 - 148 °C | ASTM D3418 |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 6800 - 7800 Pa·s Show Supplier Material materials with Melt viscosity of 6800 - 7800 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Lithium Ion Battery Binder,Lithium ion Battery Separator Coating |