Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Kynar Flex® PPA 2200
Kynar Flex® resins are fluorinated thermoplastic copolymers.
Kynar Flex® PPA 2200 resin is specially designed pellet used as a polymer process aid (PPA) for polyolefins. The use of Kynar Flex® PPA 2200 resin at 200-1000 ppm levels reduces extruder pressure, improves surface finish, reduces die build up, and improves gauge control.
Diese Materialdaten wurden von Arkema Technical Polymers zur Verfügung gestellt
All categories
Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 0.7 g/cm³ Show Supplier Material materials with Dichte of 0.7 g/cm³ | dry | ISO 1183 |
Schüttdichte | 0.6 - 0.8 g/cm³ Show Supplier Material materials with Schüttdichte of 0.6 - 0.8 g/cm³ |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 144 °C Show Supplier Material materials with Schmelzpunkt of 144 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Fluoropolymer Processing Aids |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.