Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 0.7 g/cm³ Show Supplier Material materials with Dichte of 0.7 g/cm³ | dry | ISO 1183 |
Schüttdichte | 0.5 - 0.9 g/cm³ Show Supplier Material materials with Schüttdichte of 0.5 - 0.9 g/cm³ |
Mechanisch
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 165 °C Show Supplier Material materials with Schmelzpunkt of 165 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Fluoropolymer Processing Aids |