Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 0.7 g/cm³ Show Supplier Material materials with Dichte of 0.7 g/cm³ | dry | ISO 1183 |
Schüttdichte | 0.5 - 0.9 g/cm³ Show Supplier Material materials with Schüttdichte of 0.5 - 0.9 g/cm³ |
Mechanisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Streckgrenze | 15 MPa Show Supplier Material materials with Streckgrenze of 15 MPa | dry | ISO 527-1/-2 |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Fluoropolymer Processing Aids |