Allgemein
Property | Value | Testing Standard | Condition |
---|---|---|---|
Dichte | 1.77 - 1.79 g/cm³ Show Supplier Material materials with Dichte of 1.77 - 1.79 g/cm³ | ASTM D792 | |
1.77 g/cm³ Show Supplier Material materials with Dichte of 1.77 g/cm³ | ISO 1183 | dry | |
Moisture absorption | 0.015 % Show Supplier Material materials with Moisture absorption of 0.015 % | Sim. to ISO 62 | |
Sauerstoffindex | 60 % Show Supplier Material materials with Sauerstoffindex of 60 % | ASTM D2863 | |
83 % Show Supplier Material materials with Sauerstoffindex of 83 % | ISO 4589-1/-2 | dry | |
Wasserabsorption | 0.01 - 0.03 % Show Supplier Material materials with Wasserabsorption of 0.01 - 0.03 % | ASTM D570 | |
0.03 % Show Supplier Material materials with Wasserabsorption of 0.03 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Biegemodul | 1.4 - 2.3 GPa Show Supplier Material materials with Biegemodul of 1.4 - 2.3 GPa | ASTM D790 | |||
Dehnung | 20 - 100 % Show Supplier Material materials with Dehnung of 20 - 100 % | ASTM D638 | |||
50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527-1/-2 | dry | min. | nominal | ||
Druckfestigkeit | 68.9 - 103 MPa Show Supplier Material materials with Druckfestigkeit of 68.9 - 103 MPa | ASTM D695 | |||
Elastizitätsmodul | 2 GPa Show Supplier Material materials with Elastizitätsmodul of 2 GPa | ISO 527-1/-2 | dry | ||
Elongation at yield | 9 % Show Supplier Material materials with Elongation at yield of 9 % | ISO 527-1/-2 | dry | ||
Härte, Shore D | 76 - 80 [-] Show Supplier Material materials with Härte, Shore D of 76 - 80 [-] | ASTM D2240 | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179/1eA | dry | |
23 °C | 22 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 22 kJ/m² | ISO 179/1eA | dry | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | ISO 179/1eU | dry | ||
Streckgrenze | 44.8 - 55.2 MPa Show Supplier Material materials with Streckgrenze of 44.8 - 55.2 MPa | ASTM D638 | |||
Zugfestigkeit | 34.5 - 55.2 MPa Show Supplier Material materials with Zugfestigkeit of 34.5 - 55.2 MPa | ASTM D638 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | dry | ASTM D7028, ISO 11357-1/-2 | 10°C/min | |||||
Koeffizient der thermischen Ausdehnung | 0.000119 - 0.000144 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000119 - 0.000144 1/K | ASTM D696 | |||||||
0.00015 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00015 1/K | dry | ISO 11359-1/-2 | |||||||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | UL 746B | |||||||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | UL 746B | |||||||
Schmelzpunkt | 169 °C Show Supplier Material materials with Schmelzpunkt of 169 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
172 °C Show Supplier Material materials with Schmelzpunkt of 172 °C | ASTM D3418 | ||||||||
Spezifische Wärmekapazität | 745 - 958 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 745 - 958 J/(kg·K) | DSC | |||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Vicat-Erweichungstemperatur | 138 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 138 °C | ISO 306 | 50°C/h 50N | ||||||
Wärmeformbeständigkeitstemperatur | 104 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 104 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
105 - 115 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 105 - 115 °C | ASTM D648 | 2 MPa | 248 °F/hr | ||||||
125 - 140 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 125 - 140 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
Wärmeleitfähigkeit | 0.17 - 0.19 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.17 - 0.19 W/(m·K) | ASTM D433 | |||||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7 [-] | dry | 1MHz | IEC 60250 |
10.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 10.5 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 27 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 27 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Surface resistivity | 4e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 4e+13 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.027 [-] Show Supplier Material materials with Verlustfaktor of 0.027 [-] | dry | 100Hz | IEC 60250 |
0.24 [-] Show Supplier Material materials with Verlustfaktor of 0.24 [-] | dry | 1MHz | IEC 60250 | |
Volume resistivity | 2.3e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 2.3e+12 Ω·cm | dry | IEC 60093 | |
2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | 65% RH | ASTM D257 |
Optisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Brechungsindex | 1 [-] Show Supplier Material materials with Brechungsindex of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 1500 - 2000 Pa·s Show Supplier Material materials with Melt viscosity of 1500 - 2000 Pa·s | ASTM D3835 | ||
Schmelzmassenflussrate | 1 - 3 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 1 - 3 g/10min | ASTM D1238 | 230°C/5kg | |
Schmelzvolumenflussrate | 1.1 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 1.1 cm³/10min | ISO 1133 | dry | 230°C/5kg |
Schrumpfung | 2 % Show Supplier Material materials with Schrumpfung of 2 % | ISO 294-4 | dry | |
2 % Show Supplier Material materials with Schrumpfung of 2 % | ISO 294-4 | dry | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry,Chemical Process Industry - High Purity Piping,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Plenum Pipe,Tubing and Hoses |