Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | dry | ISO 1183 |
1.84 - 1.88 g/cm³ Show Supplier Material materials with Dichte of 1.84 - 1.88 g/cm³ | ASTM D792 | ||
Sauerstoffindex | 43 % Show Supplier Material materials with Sauerstoffindex of 43 % | dry | ISO 4589-1/-2 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 40 % Show Supplier Material materials with Dehnung of 40 % | dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.6 GPa Show Supplier Material materials with Elastizitätsmodul of 1.6 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA | ||
Streckgrenze | 45 MPa Show Supplier Material materials with Streckgrenze of 45 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Schmelzpunkt | 165 - 172 °C Show Supplier Material materials with Schmelzpunkt of 165 - 172 °C | ASTM D3418 | ||
166 °C Show Supplier Material materials with Schmelzpunkt of 166 °C | ISO 11357-1/-3 | dry | 10°C/min |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 0.07 [-] Show Supplier Material materials with Dielektrizitätskonstante of 0.07 [-] | dry | 100Hz | IEC 60250 |
Durchschlagfestigkeit | 27 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 27 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 10000 Ω/sq Show Supplier Material materials with Surface resistivity of 10000 Ω/sq | cond. | IEC 60093 | |
Volume resistivity | 1e+06 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+06 Ω·cm | dry | IEC 60093 |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 2500 Pa·s Show Supplier Material materials with Melt viscosity of 2500 Pa·s | ASTM D3835 | ||
Schmelzmassenflussrate | 3 - 8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 3 - 8 g/10min | ASTM D1238 | 230°C/10kg | |
Schmelzvolumenflussrate | 4 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 4 cm³/10min | ISO 1133 | dry | 230°C/10kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - In-Tank and Fuel Venting Lines,Chemical Process Industry,Chemical Process Industry - Stock Shapes,Permanent Antistatic Solutions | |
Fillers | Carbon Black |