Allgemein
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Coefficient of friction | 0.17 [-] Show Supplier Material materials with Coefficient of friction of 0.17 [-] | ASTM D1894 | vs Steel, Kinetic | |
0.23 [-] Show Supplier Material materials with Coefficient of friction of 0.23 [-] | ASTM D1894 | vs Steel, Static | ||
Dichte | 1.75 - 1.77 g/cm³ Show Supplier Material materials with Dichte of 1.75 - 1.77 g/cm³ | ASTM D792 | ||
1.76 g/cm³ Show Supplier Material materials with Dichte of 1.76 g/cm³ | ISO 1183 | dry | ||
Sauerstoffindex | 43 % Show Supplier Material materials with Sauerstoffindex of 43 % | ISO 4589-1/-2 | dry | |
44 % Show Supplier Material materials with Sauerstoffindex of 44 % | ASTM D2863 | |||
Wasserabsorption | 0.04 % Show Supplier Material materials with Wasserabsorption of 0.04 % | Sim. to ISO 62, ASTM D570 | max. |
Mechanisch
Property | Temperature | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 48.3 - 62.1 MPa Show Supplier Material materials with Biegefestigkeit of 48.3 - 62.1 MPa | ASTM D790 | at 5% strain | ||
Biegemodul | 1.4 - 1.8 GPa Show Supplier Material materials with Biegemodul of 1.4 - 1.8 GPa | ASTM D790 | |||
Dehnung | 50 - 250 % Show Supplier Material materials with Dehnung of 50 - 250 % | ASTM D638 | |||
50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527-1/-2 | dry | min. | nominal | ||
Druckfestigkeit | 55.2 - 68.9 MPa Show Supplier Material materials with Druckfestigkeit of 55.2 - 68.9 MPa | ASTM D695 | |||
Elastizitätsmodul | 1.0 - 1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.0 - 1.4 GPa | ASTM D638 | |||
1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 GPa | ISO 527-1/-2 | dry | |||
Elongation at yield | 10 - 15 % Show Supplier Material materials with Elongation at yield of 10 - 15 % | ASTM D638 | |||
13 % Show Supplier Material materials with Elongation at yield of 13 % | ISO 527-1/-2 | dry | |||
Härte, Shore D | 75 - 80 [-] Show Supplier Material materials with Härte, Shore D of 75 - 80 [-] | ASTM D2240 | |||
Impact strength, Charpy notched, ASTM | 23 °C | 96.1 - 214 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 96.1 - 214 J/m | ASTM D256 | ||
Impact strength, Charpy unnotched, ASTM | 23 °C | 801 - 2140 J/m Show Supplier Material materials with Impact strength, Charpy unnotched, ASTM of 801 - 2140 J/m | ASTM D256 | ||
Streckgrenze | 34.5 - 51.7 MPa Show Supplier Material materials with Streckgrenze of 34.5 - 51.7 MPa | ASTM D638 | |||
52 MPa Show Supplier Material materials with Streckgrenze of 52 MPa | ISO 527-1/-2 | dry | |||
Zugfestigkeit | 31 - 48.3 MPa Show Supplier Material materials with Zugfestigkeit of 31 - 48.3 MPa | ASTM D638 |
Thermisch
Property | Value | Testing Standard | Condition | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -40.6 - -38.3 °C Show Supplier Material materials with Glasübergangstemperatur of -40.6 - -38.3 °C | ASTM D7028 | |||||||
-40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | ISO 11357-1/-2 | dry | 10°C/min | ||||||
Koeffizient der thermischen Ausdehnung | 9e-05 - 0.000126 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-05 - 0.000126 1/K | ASTM D696 | |||||||
Schmelzpunkt | 155 - 172 °C Show Supplier Material materials with Schmelzpunkt of 155 - 172 °C | ASTM D3418 | |||||||
161 °C Show Supplier Material materials with Schmelzpunkt of 161 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Spezifische Wärmekapazität | 745 - 958 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 745 - 958 J/(kg·K) | DSC | |||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Wärmeformbeständigkeitstemperatur | 80 - 90 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 80 - 90 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
85 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 85 °C | ISO 75-1/-2 | dry | 2 MPa | ||||||
112 - 140 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 112 - 140 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
Wärmeleitfähigkeit | 0.17 - 0.19 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.17 - 0.19 W/(m·K) | ASTM D433 | |||||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Elektrisch
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Dielektrizitätskonstante | 4.5 - 9.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.5 - 9.5 [-] | 1KHz | ASTM D150 | |
6.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 6.7 [-] | 1MHz | IEC 60250 | dry | |
9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 9 [-] | 100Hz | IEC 60250 | dry | |
Durchschlagfestigkeit | 63 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 63 kV/mm | ASTM D149, IEC 60243-1 | dry | |
Surface resistivity | 5.1e+11 - 5.3e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 5.1e+11 - 5.3e+11 Ω/sq | ASTM D257 | ||
Verlustfaktor | 0.01 - 0.21 [-] Show Supplier Material materials with Verlustfaktor of 0.01 - 0.21 [-] | 100KHz | ASTM D150 | |
0.07 [-] Show Supplier Material materials with Verlustfaktor of 0.07 [-] | 1MHz | IEC 60250 | dry | |
0.13 [-] Show Supplier Material materials with Verlustfaktor of 0.13 [-] | 100Hz | IEC 60250 | dry | |
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH | |
2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | IEC 60093 | dry |
Optisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Brechungsindex | 1 [-] Show Supplier Material materials with Brechungsindex of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 2350 - 2950 Pa·s Show Supplier Material materials with Melt viscosity of 2350 - 2950 Pa·s | ASTM D3835 | ||
Schmelzmassenflussrate | 6 - 14 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 6 - 14 g/10min | ASTM D1238 | 230°C/21.6kg | |
Schmelzvolumenflussrate | 5.6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 5.6 cm³/10min | ISO 1133 | dry | 230°C/21.6kg |
Schrumpfung | 2 % Show Supplier Material materials with Schrumpfung of 2 % | ISO 294-4 | dry | |
2 % Show Supplier Material materials with Schrumpfung of 2 % | ISO 294-4 | dry | Transverse | |
Thermal conductivity of melt | 0.19 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.19 W/(m·K) |