Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.77 g/cm³ Show Supplier Material materials with Dichte of 1.77 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.015 % Show Supplier Material materials with Moisture absorption of 0.015 % | Sim. to ISO 62 | |
Sauerstoffindex | 80 % Show Supplier Material materials with Sauerstoffindex of 80 % | dry | ISO 4589-1/-2 |
Wasserabsorption | 0.02 % Show Supplier Material materials with Wasserabsorption of 0.02 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 40 % Show Supplier Material materials with Dehnung of 40 % | dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 9 % Show Supplier Material materials with Elongation at yield of 9 % | dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | dry | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 221 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 221 kJ/m² | dry | ISO 179/1eU | |
23 °C | 227 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 227 kJ/m² | dry | ISO 179/1eU | ||
Streckgrenze | 54 MPa Show Supplier Material materials with Streckgrenze of 54 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | dry | ISO 11357-1/-2 | 10°C/min | |||||
Koeffizient der thermischen Ausdehnung | 0.00015 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00015 1/K | dry | ISO 11359-1/-2 | ||||||
Schmelzpunkt | 171 °C Show Supplier Material materials with Schmelzpunkt of 171 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Vicat-Erweichungstemperatur | 140 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 140 °C | ISO 306 | 50°C/h 50N | ||||||
Wärmeformbeständigkeitstemperatur | 108 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 108 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7 [-] | dry | 1MHz | IEC 60250 |
9.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 9.5 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 24 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 24 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Surface resistivity | 1.5e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1.5e+14 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.028 [-] Show Supplier Material materials with Verlustfaktor of 0.028 [-] | dry | 100Hz | IEC 60250 |
0.22 [-] Show Supplier Material materials with Verlustfaktor of 0.22 [-] | dry | 1MHz | IEC 60250 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | dry | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 6.7 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 6.7 cm³/10min | dry | ISO 1133 | 230°C/5kg |
Schrumpfung | 2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | ISO 294-4 | |
2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes | |
Processing methods | Injection Molding: |