Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | dry | ISO 1183 |
Sauerstoffindex | 42 % Show Supplier Material materials with Sauerstoffindex of 42 % | dry | ISO 4589-1/-2 |
Wasserabsorption | 0.008 % Show Supplier Material materials with Wasserabsorption of 0.008 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 2 GPa Show Supplier Material materials with Elastizitätsmodul of 2 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 9 % Show Supplier Material materials with Elongation at yield of 9 % | dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 36 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 36 kJ/m² | dry | ISO 179/1eA | |
Streckgrenze | 50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | dry | ISO 11357-1/-2 | 10°C/min | |||||
Koeffizient der thermischen Ausdehnung | 0.00015 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00015 1/K | dry | ISO 11359-1/-2 | ||||||
Schmelzpunkt | 169 °C Show Supplier Material materials with Schmelzpunkt of 169 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Wärmeformbeständigkeitstemperatur | 104 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 104 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: V-0 and yellow card available |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 1.4 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 1.4 cm³/10min | dry | ISO 1133 | 230°C/3.8kg |
Schrumpfung | 2.5 % Show Supplier Material materials with Schrumpfung of 2.5 % | dry | ISO 294-4 | |
2.5 % Show Supplier Material materials with Schrumpfung of 2.5 % | dry | ISO 294-4 | Transverse | |
Thermal conductivity of melt | 0.19 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.19 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Potable Water Distribution | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: |