Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.07 % Show Supplier Material materials with Moisture absorption of 0.07 % | Sim. to ISO 62 | |
Sauerstoffindex | 44 % Show Supplier Material materials with Sauerstoffindex of 44 % | dry | ISO 4589-1/-2 |
Wasserabsorption | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | min. | nominal |
Elastizitätsmodul | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | dry | ISO 527-1/-2 | |
Streckgrenze | 52 MPa Show Supplier Material materials with Streckgrenze of 52 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | dry | ISO 11357-1/-2 | 10°C/min | |||||
Koeffizient der thermischen Ausdehnung | 0.00015 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00015 1/K | dry | ISO 11359-1/-2 | ||||||
Schmelzpunkt | 169 °C Show Supplier Material materials with Schmelzpunkt of 169 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Vicat-Erweichungstemperatur | 139 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 139 °C | ISO 306 | 50°C/h 50N | ||||||
Wärmeformbeständigkeitstemperatur | 110 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 110 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
132 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 132 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||||||
Entflammbarkeit | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard | Comment |
---|---|---|---|---|---|
Dielektrizitätskonstante | 7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7 [-] | dry | 1MHz | IEC 60250 | |
9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 9 [-] | dry | 100Hz | IEC 60250 | ||
Durchschlagfestigkeit | 21 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 21 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | ||
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | cond. | IEC 60093 | min. | |
Verlustfaktor | 0.032 [-] Show Supplier Material materials with Verlustfaktor of 0.032 [-] | dry | 100Hz | IEC 60250 | |
0.214 [-] Show Supplier Material materials with Verlustfaktor of 0.214 [-] | dry | 1MHz | IEC 60250 | ||
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | dry | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 27 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 27 cm³/10min | dry | ISO 1133 | 230°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Metal Tube Coating |