Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | dry | ISO 527-1/-2 | |
Streckgrenze | 42 MPa Show Supplier Material materials with Streckgrenze of 42 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Schmelzpunkt | 165 °C Show Supplier Material materials with Schmelzpunkt of 165 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Wärmeformbeständigkeitstemperatur | 72 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 72 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
Entflammbarkeit | At thickness 0.8 mm IEC 60695-11-10: HB |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry,Underground Fuel Containment |