Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.77 g/cm³ Show Supplier Material materials with Dichte of 1.77 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | Sim. to ISO 62 | |
Wasserabsorption | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 46 % Show Supplier Material materials with Dehnung of 46 % | dry | ISO 527-1/-2 | min. | nominal |
Elastizitätsmodul | 1.5 GPa Show Supplier Material materials with Elastizitätsmodul of 1.5 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | dry | ISO 527-1/-2 | |
Streckgrenze | 45 MPa Show Supplier Material materials with Streckgrenze of 45 MPa | dry | ISO 527-3 |
Thermisch
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 6.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 6.5 [-] | dry | 1MHz | IEC 60250 |
10.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 10.5 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 21 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 21 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.038 [-] Show Supplier Material materials with Verlustfaktor of 0.038 [-] | dry | 100Hz | IEC 60250 |
0.234 [-] Show Supplier Material materials with Verlustfaktor of 0.234 [-] | dry | 1MHz | IEC 60250 | |
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | dry | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 25 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 25 cm³/10min | dry | ISO 1133 | 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Metal Tube Coating,Chemical Process Industry,Chemical Process Industry - Coating of Chemical Pumps,Chemical Process Industry - Coating of Chemical Valves,Chemical Process Industry - Coating of Chemical Vessels |