Allgemein
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-3 | Transverse |
100 % Show Supplier Material materials with Dehnung of 100 % | dry | ISO 527-3 | ||
Elongation at yield | 11 % Show Supplier Material materials with Elongation at yield of 11 % | dry | ISO 527-3 | |
Elongation at yield, transverse | 11 % Show Supplier Material materials with Elongation at yield, transverse of 11 % | dry | ISO 527-3 | |
Reißfestigkeit | 2 kN/m Show Supplier Material materials with Reißfestigkeit of 2 kN/m | ISO 6383-1 | ||
3 kN/m Show Supplier Material materials with Reißfestigkeit of 3 kN/m | ISO 6383-1 | Transverse | ||
Zugfestigkeit | 30 MPa Show Supplier Material materials with Zugfestigkeit of 30 MPa | dry | ISO 527-3 | Transverse |
30 MPa Show Supplier Material materials with Zugfestigkeit of 30 MPa | dry | ISO 527-3 |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 110 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 110 kV/mm | dry | IEC 60243-1 |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic / Solar Film |