Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.36 g/cm³ Show Supplier Material materials with Dichte of 1.36 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-3 | Transverse |
50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-3 | ||
Elongation at yield | 3.5 % Show Supplier Material materials with Elongation at yield of 3.5 % | dry | ISO 527-3 | |
Elongation at yield, transverse | 3.5 % Show Supplier Material materials with Elongation at yield, transverse of 3.5 % | dry | ISO 527-3 | |
Reißfestigkeit | 2 kN/m Show Supplier Material materials with Reißfestigkeit of 2 kN/m | ISO 6383-1 | ||
3 kN/m Show Supplier Material materials with Reißfestigkeit of 3 kN/m | ISO 6383-1 | Transverse | ||
Zugfestigkeit | 25 MPa Show Supplier Material materials with Zugfestigkeit of 25 MPa | dry | ISO 527-3 | Transverse |
30 MPa Show Supplier Material materials with Zugfestigkeit of 30 MPa | dry | ISO 527-3 |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 100 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 100 kV/mm | dry | IEC 60243-1 |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic / Solar Film |