Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Kynar® HSV 1800
Kynar® resins are fluorinated thermoplastic polymers, specially designed to bring a high level of adhesion even at a very low binder content. This binder can be used for cathode and anode formulation.
Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo mechanical properties.
Diese Materialdaten wurden von Arkema Technical Polymers zur Verfügung gestellt
All categories
Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | dry | ISO 1183 |
Technological properties
Property | ||
---|---|---|
Application areas | Lithium Ion Battery Binder |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.