Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.77 - 1.79 g/cm³ Show Supplier Material materials with Dichte of 1.77 - 1.79 g/cm³ | ASTM D792 |
Sauerstoffindex | 44 % Show Supplier Material materials with Sauerstoffindex of 44 % | ASTM D2863 |
Mechanisch
Property | Temperature | Value | Testing Standard |
---|---|---|---|
Biegemodul | 1.4 - 2.2 GPa Show Supplier Material materials with Biegemodul of 1.4 - 2.2 GPa | ASTM D790 | |
Dehnung | 50 - 250 % Show Supplier Material materials with Dehnung of 50 - 250 % | ASTM D638 | |
Druckfestigkeit | 68.9 - 103 MPa Show Supplier Material materials with Druckfestigkeit of 68.9 - 103 MPa | ASTM D695 | |
Härte, Shore D | 76 - 80 [-] Show Supplier Material materials with Härte, Shore D of 76 - 80 [-] | ASTM D2240 | |
Impact strength, Charpy notched, ASTM | 23 °C | 107 - 320 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 107 - 320 J/m | ASTM D256 |
Streckgrenze | 40 - 55.2 MPa Show Supplier Material materials with Streckgrenze of 40 - 55.2 MPa | ASTM D638 | |
Zugfestigkeit | 34 - 43 MPa Show Supplier Material materials with Zugfestigkeit of 34 - 43 MPa | ASTM D638 |
Thermisch
Property | Value | Testing Standard |
---|---|---|
Schmelzpunkt | 165 - 342 °C Show Supplier Material materials with Schmelzpunkt of 165 - 342 °C | ASTM D3418 |
Optisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Brechungsindex | 1 [-] Show Supplier Material materials with Brechungsindex of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 7000 - 7500 Pa·s Show Supplier Material materials with Melt viscosity of 7000 - 7500 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Lithium Ion Battery Binder |