Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.77 - 1.79 g/cm³ Show Supplier Material materials with Dichte of 1.77 - 1.79 g/cm³ | ASTM D792 | |
Wasserabsorption | 0.04 % Show Supplier Material materials with Wasserabsorption of 0.04 % | ASTM D570 | max. |
Mechanisch
Property | Value | Testing Standard |
---|---|---|
Biegemodul | 1.4 - 2.3 GPa Show Supplier Material materials with Biegemodul of 1.4 - 2.3 GPa | ASTM D790 |
Elastizitätsmodul | 1.4 - 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 - 2.3 GPa | ASTM D638 |
Streckgrenze | 44.8 - 55.2 MPa Show Supplier Material materials with Streckgrenze of 44.8 - 55.2 MPa | ASTM D638 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Glasübergangstemperatur | -40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | dry | ISO 11357-1/-2 | 10°C/min |
Schmelzpunkt | 162 - 172 °C Show Supplier Material materials with Schmelzpunkt of 162 - 172 °C | ASTM D3418 |
Optisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Brechungsindex | 1 [-] Show Supplier Material materials with Brechungsindex of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 4800 - 5250 Pa·s Show Supplier Material materials with Melt viscosity of 4800 - 5250 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Biopharma Membranes,Water Filtration Membrane | |
Certifications | Yellow Card - NSF, FDA, and USP Class VI certifications for use in potable water, food processing, and bio-pharma applications. |