Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.14 g/cm³ Show Supplier Material materials with Dichte of 1.14 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. |
Elastizitätsmodul | 0.572 GPa Show Supplier Material materials with Elastizitätsmodul of 0.572 GPa | cond. | ISO 527-1/-2 | |
Streckgrenze | 28 MPa Show Supplier Material materials with Streckgrenze of 28 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 215 °C Show Supplier Material materials with Schmelzpunkt of 215 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 1 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 1 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Air Conditioning Circuit | |
Processing methods | Extrusion: |