Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | |
Elastizitätsmodul | 0.5 GPa Show Supplier Material materials with Elastizitätsmodul of 0.5 GPa | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 55 [-] Show Supplier Material materials with Härte, Shore D of 55 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 21.6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 21.6 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 83 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 83 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 24 MPa Show Supplier Material materials with Streckgrenze of 24 MPa | cond. | ISO 527-1/-2 | ||
35 MPa Show Supplier Material materials with Streckgrenze of 35 MPa | dry | ISO 527-3 | |||
49 MPa Show Supplier Material materials with Streckgrenze of 49 MPa | dry | ISO 527-2/-2 |
Thermisch
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 1.1 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 1.1 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Alternative Fuel Systems - CNG, LPG, LNG Lines and Tanks | |
Processing methods | Blow Molding: |