Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | Sim. to ISO 62 | |
Wasserabsorption | 5 % Show Supplier Material materials with Wasserabsorption of 5 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | |
Elastizitätsmodul | 0.3 GPa Show Supplier Material materials with Elastizitätsmodul of 0.3 GPa | cond. | ISO 527-1/-2 | ||
0.6 GPa Show Supplier Material materials with Elastizitätsmodul of 0.6 GPa | dry | ISO 527-1/-2 | |||
Härte, Shore D | 50 [-] Show Supplier Material materials with Härte, Shore D of 50 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 80 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 80 kJ/m² | dry | ISO 179/1eA | |
23 °C | 84 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 84 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23°C | dry and cond. | ISO 179/1eU |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Vicat-Erweichungstemperatur | 62 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 62 °C | ISO 306 | 50°C/h 50N | ||||||
Wärmeformbeständigkeitstemperatur | 60 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 60 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 2.5 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 2.5 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Schrumpfung | 0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | dry | ISO 294-4 | |
0.9 % Show Supplier Material materials with Schrumpfung of 0.9 % | dry | ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Air Conditioning Circuit | |
Processing methods | Injection Molding: Extrusion: |