Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | |
Elastizitätsmodul | 0.5 GPa Show Supplier Material materials with Elastizitätsmodul of 0.5 GPa | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 55 [-] Show Supplier Material materials with Härte, Shore D of 55 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 83 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 83 kJ/m² | cond., dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23°C | dry and cond. | ISO 179/1eU | ||
Streckgrenze | 35 MPa Show Supplier Material materials with Streckgrenze of 35 MPa | dry | ISO 527-3 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00017 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00017 1/K | dry | ISO 11359-1/-2 | ||||
0.00018 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00018 1/K | dry | ISO 11359-1/-2 | Transverse | ||||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Vicat-Erweichungstemperatur | 75 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 75 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard | Comment |
---|---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | cond. | 100Hz | IEC 60250 | |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | IEC 60250 | 1MHz | |||
Durchschlagfestigkeit | 36 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 36 kV/mm | cond., dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | ||
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | cond. | IEC 60093 | min. | |
Verlustfaktor | 0.05 [-] Show Supplier Material materials with Verlustfaktor of 0.05 [-] | cond. | 1MHz | IEC 60250 | |
0.11 [-] Show Supplier Material materials with Verlustfaktor of 0.11 [-] | cond. | 100Hz | IEC 60250 | ||
Volume resistivity | 7.5e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 7.5e+11 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 1 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 1 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Air Intake Circuit | |
Processing methods | Injection Molding: Extrusion: Blow Molding: |