Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.12 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal |
Elastizitätsmodul | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | cond. | ISO 527-1/-2 | |
Elongation at yield | 4.4 % Show Supplier Material materials with Elongation at yield of 4.4 % | cond. | ISO 527-1/-2 | |
Streckgrenze | 48 MPa Show Supplier Material materials with Streckgrenze of 48 MPa | cond. | ISO 527-1/-2 | |
80 MPa Show Supplier Material materials with Streckgrenze of 80 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 229 °C Show Supplier Material materials with Schmelzpunkt of 229 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Air Conditioning Circuit | |
Processing methods | Extrusion: |