Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1 % Show Supplier Material materials with Moisture absorption of 1 % | Sim. to ISO 62 | |
Wasserabsorption | 2.3 % Show Supplier Material materials with Wasserabsorption of 2.3 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | cond., dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 8.3 GPa Show Supplier Material materials with Elastizitätsmodul of 8.3 GPa | cond. | ISO 527-1/-2 | ||
8.9 GPa Show Supplier Material materials with Elastizitätsmodul of 8.9 GPa | dry | ISO 527-1/-2 | |||
Härte, Shore D | 78 [-] Show Supplier Material materials with Härte, Shore D of 78 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 16 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | dry | ISO 179/1eA | |
23 °C | 17 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 17 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23°C | cond. | ISO 179/1eU | ||
Streckgrenze | 52 MPa Show Supplier Material materials with Streckgrenze of 52 MPa | cond. | ISO 527-1/-2 | ||
Zugfestigkeit | 130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | cond. | ISO 527-1/-2 | ||
140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.9e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.9e-05 1/K | dry | ISO 11359-1/-2 | ||||||
0.000126 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000126 1/K | dry | ISO 11359-1/-2 | Transverse | ||||||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Vicat-Erweichungstemperatur | 185 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 185 °C | ISO 306 | 50°C/h 50N | ||||||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB and yellow card available |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard | Comment |
---|---|---|---|---|---|
Dielektrizitätskonstante | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3 [-] | cond. | 100Hz | IEC 60250 | |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | IEC 60250 | 1MHz | |||
Durchschlagfestigkeit | 34 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 34 kV/mm | cond., dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | ||
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | cond. | IEC 60093 | min. | |
Verlustfaktor | 0.023 [-] Show Supplier Material materials with Verlustfaktor of 0.023 [-] | cond. | 1MHz | IEC 60250 | |
0.064 [-] Show Supplier Material materials with Verlustfaktor of 0.064 [-] | cond. | 100Hz | IEC 60250 | ||
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | cond. | IEC 60093 | min. |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 2 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 2 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Schrumpfung | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | dry | ISO 294-4 | |
0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | dry | ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors E&E | |
Certifications | Yellow Card | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding: |