Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coarse particles amount | 5 % Show Supplier Material materials with Coarse particles amount of 5 % | ISO 13319 | max. |
Coarse particles size | 10 μm Show Supplier Material materials with Coarse particles size of 10 μm | min. | |
Dichte | 0.215 g/cm³ Show Supplier Material materials with Dichte of 0.215 g/cm³ | ISO 1068 | apparent density unpacked |
Fine particles amount | 2 % Show Supplier Material materials with Fine particles amount of 2 % | ISO 13319 | max. |
Fine particles size | 2.5 μm Show Supplier Material materials with Fine particles size of 2.5 μm | max. | |
Median particles size | 5 μm Show Supplier Material materials with Median particles size of 5 μm | ISO 13319 | |
Spezifische Oberfläche | 9 m²/g Show Supplier Material materials with Spezifische Oberfläche of 9 m²/g | ISO 9277 |
Thermisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Schmelzpunkt | 177 °C Show Supplier Material materials with Schmelzpunkt of 177 °C | dry | ISO 11357-3 |
Technological properties
Property | ||
---|---|---|
Application areas | Coating Additives,Coating Additives - Floor Coating,Coating Additives - Wood Coating,Coating Additives - Inks-OPVs |