Property | Value | Testing Standard | Comment |
---|---|---|---|
Coarse particles amount | 5 % Show Supplier Material materials with Coarse particles amount of 5 % | ISO 13319 | max. |
Coarse particles size | 80 μm Show Supplier Material materials with Coarse particles size of 80 μm | min. | |
Dichte | 0.425 g/cm³ Show Supplier Material materials with Dichte of 0.425 g/cm³ | ISO 1068 | apparent density unpacked |
Fine particles amount | 10 % Show Supplier Material materials with Fine particles amount of 10 % | ISO 13319 | max. |
Fine particles size | 40 μm Show Supplier Material materials with Fine particles size of 40 μm | max. | |
Median particles size | 60 μm Show Supplier Material materials with Median particles size of 60 μm | ISO 13319 | |
Spezifische Oberfläche | 1 m²/g Show Supplier Material materials with Spezifische Oberfläche of 1 m²/g | ISO 9277 |
Thermisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Schmelzpunkt | 177 °C Show Supplier Material materials with Schmelzpunkt of 177 °C | dry | ISO 11357-3 |
Technological properties
Property | ||
---|---|---|
Application areas | Coating Additives,Coating Additives - Coil Coating |