Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1 g/cm³ Show Supplier Material materials with Dichte of 1 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | Sim. to ISO 62 | |
Wasserabsorption | 1.2 % Show Supplier Material materials with Wasserabsorption of 1.2 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. |
Elastizitätsmodul | 0.01 GPa Show Supplier Material materials with Elastizitätsmodul of 0.01 GPa | cond. | ISO 527-1/-2 | |
0.012 GPa Show Supplier Material materials with Elastizitätsmodul of 0.012 GPa | dry | ISO 527-1/-2 | ||
Härte, Shore A | 77 [-] Show Supplier Material materials with Härte, Shore A of 77 [-] | ISO 7619-1 | for 3 seconds | |
Härte, Shore D | 22 [-] Show Supplier Material materials with Härte, Shore D of 22 [-] | dry | ISO 7619-1 | 15 seconds |
Schlagfestigkeit, Charpy gekerbt | No Break at 23 and -30°C | dry and cond. | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Conveyor Belts and Pulleys | |
Certifications | Food Contact | |
Processing methods | Injection Molding: |